Friday, June 17, 2011

Application of liquid wallpaper.

Deposition of liquid wallpaper is simple and accessible to everyone. The most important stage for a qualitative application of liquid wallpaper is to prepare the work surface. Necessary to complete removal of old wallpaper, glue stains, etc. Liquid wallpaper can be applied to plaster walls, the walls are painted with oil-or water-dispersion paint. Metal parts must be primed with enamel or oil paint, plastic and plastikovidnye surface - water-dispersion paint with the addition of PVA glue in the amount of 10-15% of its amount. If the existing coating has an intense color, in order to avoid its manifestation outward through the damage of the liquid wallpaper must be a primer to use waterproof formulations (specific primer, oil paint, enamel, etc.) and priming carried out in two layers. In the next stage (after drying primer) the source material - a dry track - mixed thoroughly in a plastic container with water, added gradually in portions, to obtain a homogeneous mass with the consistency of thick cream. In this case, the solution was removed from the large inclusions of the material. To expedite the preparation of liquid wallpaper using warm water with temperatures around 25 ° C. After this batch is aged for 15-20 minutes before applying again mixed. To get the perfect uniformity of color coating solution was prepared simultaneously from multiple packages. To personalize the interior of a mixture of liquid wallpaper adds various decorative additions. All prepared for the work surface should be covered in one step. Therefore, the necessary amount of material necessary to prepare in advance. Application of liquid wallpaper by using pnevmoraspylitelnogo gun or by hand - using a plastic trowel or a paint roller with a hard coat. When spraying gun should be used with the compressor working pressure 0,4-0,5 MPa and productivity at least 400 l / min section of the nozzle gun - 5, 7, 10 mm depending on the texture of the applied coating type. Optimal flow when spraying is achieved by varying the amount of water introduced into the material. Performance of 25-45 m2 / h. In the case of drawing a pistol, first applied to a small layer that covers the wall vsploshnuyu. After drying, it is a final coating with the desired thickness. If the coat pnevmoraspylitelem in one step, then the normal density of coverage in some parts of the wall may creep cover during spraying. In case of application of hand-made throwing mortar on the wall in small portions and the leveling of the paint roller with a hard coat or a flattening of arbitrary motion with a plastic float. Textured finish by using embossed rolls. Rolling pattern produced after 4-8 hours after application to the surface of liquid obsev. In the process of drawing roller regularly moistened with water. Versatility of the material allows, in some cases do without plastering. Brickwork, tiles, plasterboard, particleboard, and other surfaces are covered in two phases. First, liquid wallpaper shpatlyuyut seams. Then, after drying, applied to the second, the decorative layer. Can not be left unfinished surface. Suspension of work should be completed before the setting material. Should not be applied liquid wallpaper in rooms with temperatures below 10 ° C. Damage layer takes its final shape and color after drying. For fastest drying liquid wallpaper desirable indoor conditions of good ventilation (as opposed to the drying process of conventional wallpaper). Drying time in a well ventilated area with temperatures around 20 ° C - 1 to 3 days. Depending on the condition of the surface of one kilogram of dry mixture can be covered up to 2-3 m2 of surface. Durability covers 10 years. When carrying out repair work damage or contamination of the wall coating is wetted with water, removed and then erased the newly prepared compound. When cosmetic repair coverage is enough to refresh the water-dispersion paint with any dye carrier. If the coating you are tired or you do something changed in the environment and you do not fit the color or texture, crashes moistened and gently remove with a spatula, soaked in water and then applied to another surface.

No comments:

Post a Comment